Temperature Stressing Figures
Figure 1
Plot showing reduction in IDDQ after a 16 hour unbiased bake at 150°C (Courtesy Sandia Labs)

Figure 2
Plot showing reduction in IDDQ after two differing unbiased bakes (Courtesy Sandia Labs)

Figure 3
Plot showing an increase in IDDQ after biased temperature stressing (Courtesy Sandia Labs)

Figure 4
Plot showing an increase in IDDQ after two biased temperature stresses (Courtesy Sandia Labs)